Product Introduction
3160 Micronized Wax
Chemical Composition Polyethylene wax
Typical Materialized Data
The data presented on this data page are only typical values, not technical indicators of the product.
Melting point: |
120℃ |
Particle size distribution: |
D50:6μm D90:10μm |
Supply form: |
micro powder material |
Storage and Transportation Store in a cool,dry,and ventilated place.
Used for UV,solvent-based coatings and powdercoatings,and it has excellent transparency,slip and scratch resistance in the coating.
Application Area
Liquid Coatings and Oil Inks
Product Features and Advantages:This additive can increase surface smoothness and significantly improve scratch resistance in UVand solvent-based coatings and inks,while also providinghigh transparency and good dispersibility.
Recommended Use:Furniture coatings,floor coatings,industrial coatings,printinginks,UVcoatings, plastic coatings,tin plate coatings,and roofing coatings.
Suggested Dosage:The dosage of0.3-3%additivesis based on the totalformula,due to different formulation and process conditions,it is recommended to determine the optimal addition amount through experiment before use.
Add Method and Processing Guidance:The product can be dispersed in the paintand ink by high-speed mixing or grinding, and can also be prepared into waxand added after preparation.
Powder Coating
Features and Advantages:This additive can improve the surface smoothness and scratch resistance,and improve the surface protection of powder coating.
Suggested Dosage:The 0.3-0.6%additives are based on the total formulation,and due to the different formulation and process conditions,itis recommended to determine the optimal addition amountthrough experiments before use.
Add Method and Processing Guidance:It is recommended to add the base material when pre-mixed,and then squeeze all the material.It can also be added to the material mix with grinding sieve,or added to the finished powder mixed sieve.